I'm wondering if anyone on here have or had any problems with PM Research 4% silver-tin alloy solder and flux. on their boilers?
Asking for a friend.
I have personally built PM Research boiler #1 back in 2000 and PM Research boiler #2 in 2008 and to this date they have not failed. (hydrostatic tested each year to a pressure of 120 psi / 8.27371 bar steamed at 50 psi / 3.44738 bar ) # 1 boiler is 23 years old # 2 is 15 years old.
I am concerned because it has been mentioned that solders containing tin lose too much strength at the temperature of steam at 15psi.
Asking for a friend.
I have personally built PM Research boiler #1 back in 2000 and PM Research boiler #2 in 2008 and to this date they have not failed. (hydrostatic tested each year to a pressure of 120 psi / 8.27371 bar steamed at 50 psi / 3.44738 bar ) # 1 boiler is 23 years old # 2 is 15 years old.
I am concerned because it has been mentioned that solders containing tin lose too much strength at the temperature of steam at 15psi.