Thanks for the comments Barrie,
Although I am resigned to go the aluminium option (I have machined/fettled one at the moment), I will give your suggestions a try and see how it prints.
I did consider doing a lost PLA casting from the 3D print which is a technique I have used quite a bit and you can dress out the layer lines easier on metal.
I did look up the Ether/Paraffin resistance on Google and it indicated it was ok to use. I have just popped a sample into some fuel to confirm
Thanks for the note on CF filled PLA, I will check it out.
Cheers
Rich
Although I am resigned to go the aluminium option (I have machined/fettled one at the moment), I will give your suggestions a try and see how it prints.
I did consider doing a lost PLA casting from the 3D print which is a technique I have used quite a bit and you can dress out the layer lines easier on metal.
I did look up the Ether/Paraffin resistance on Google and it indicated it was ok to use. I have just popped a sample into some fuel to confirm
Thanks for the note on CF filled PLA, I will check it out.