aonemarine
Well-Known Member
- Joined
- Nov 18, 2012
- Messages
- 887
- Reaction score
- 212
WOW! Those casting are amazing. That what I am shooting for. I did use wax on my casting but only as a filler. Look's like more time spent on the mold before pouring. Question what type of foam did you use? I used Styrofoam the stuff that you're TV and Electronics come in. I used a hot wire to cut the foam but it seem to leave a poor result on the mold. I am going to have to start to account for lost after the casting is completed. But like I said before there's a learning curve.
He uses the pink insulation type foam then coats it with drywall mud. Once dry its bedded in sand then the aluminum is poured. Kelly, the guy who cast the above parts makes it look real easy...