jack620
Well-Known Member
My ML Midge plans call for drill rod to be used for the wrist pin. I'm not having any luck sourcing it from my local steel suppliers. Looks like an eBay job. Is this silver steel the same as drill rod?
http://www.ebay.com.au/itm/350603589931?ssPageName=STRK:MEWAX:IT&_trksid=p3984.m1423.l2648#ht_1080wt_1114
According to the manufacturer, it can be hardened by heating to 770-790C and quenching in water. My pistons have been reamed to 2.5mm, so I guess I will need to buy the rod in something larger and turn it to a press fit?
Chris
http://www.ebay.com.au/itm/350603589931?ssPageName=STRK:MEWAX:IT&_trksid=p3984.m1423.l2648#ht_1080wt_1114
According to the manufacturer, it can be hardened by heating to 770-790C and quenching in water. My pistons have been reamed to 2.5mm, so I guess I will need to buy the rod in something larger and turn it to a press fit?
Chris